Filament for drone and robot parts: stiff per gram, soft where it hits
For a drone arm, a frame plate or a robot bracket that must not flex, we print PPA-CF: on Bambu Lab's datasheets it gives 4.9 times the bending stiffness per gram of PETG HF along the layers, at almost the same weight per volume. For bumpers, feet and mounts, TPU: TPU for AMS to keep its shape, TPU 95A HF to stretch across its layers. PPA-CF and TPU for AMS are among our most popular materials, printed from one part and posted to the Baltics, Finland, Sweden and Denmark.
- PPA-CF: 4.9 times PETG HF's bending stiffness per gram along the layers
- Not lighter: PPA-CF, PPS-CF and PET-CF 1.25 to 1.29 g/cm³, PETG HF 1.28
- PPA-CF, PET-CF, ASA Aero and TPU for AMS 2-5 working days after payment
- Up to 340 x 320 x 340 mm in one piece in carbon fibre
Which filament for drone and robot parts?
Arms, frame plates and brackets that must not flex: PPA-CF, 4.9 times PETG HF's stiffness per gram along the layers. PET-CF when the part flies in the wet and need not be the stiffest.
Shells, canopies and covers, where the shape is fixed and grams count: ASA Aero, the lightest grade here at 0.99 g/cm³. Bumpers, feet and damping mounts: TPU for AMS when the part should keep its shape, TPU 95A HF when it must stretch or squeeze.
We do not certify parts for flight.
Stiffness per gram, from the datasheets

An arm is a beam in bending, so the column to read is bending modulus (ISO 178), not tensile strength. Figures are Bambu Lab's datasheet values for printed specimens, given "for design reference and comparison only". X-Y is along the layers, Z across them. The per-gram column is derived: bending modulus divided by density, shown relative to PETG HF, which is 1.0 in both directions.
| Our status | Density (ISO 1183) | Bending modulus X-Y / Z (ISO 178) | Stiffness per gram X-Y / Z, PETG HF = 1.0 | Impact X-Y / Z (ISO 179, unnotched) | Heat deflection, 1.8 MPa (ISO 75) | |
|---|---|---|---|---|---|---|
| PPA-CF | Our statusmost popular | Density (ISO 1183)1.25 g/cm³ | Bending modulus X-Y / Z (ISO 178)9,860 / 3,240 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.04.9 / 1.8 | Impact X-Y / Z (ISO 179, unnotched)41.7 / 4.3 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)196 °C |
| PPS-CF | Our statusmost popular | Density (ISO 1183)1.26 g/cm³ | Bending modulus X-Y / Z (ISO 178)7,160 / 2,460 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.03.5 / 1.4 | Impact X-Y / Z (ISO 179, unnotched)27.8 / 2.8 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)235 °C |
| PA6-CF | Our statusordered in | Density (ISO 1183)1.09 g/cm³ | Bending modulus X-Y / Z (ISO 178)5,460 / 2,240 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.03.1 / 1.5 | Impact X-Y / Z (ISO 179, unnotched)40.3 / 15.5 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)164 °C |
| PET-CF | Our statusmost popular | Density (ISO 1183)1.29 g/cm³ | Bending modulus X-Y / Z (ISO 178)5,320 / 2,210 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.02.6 / 1.2 | Impact X-Y / Z (ISO 179, unnotched)36.0 / 4.5 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)182 °C |
| PAHT-CF | Our statusordered in | Density (ISO 1183)1.06 g/cm³ | Bending modulus X-Y / Z (ISO 178)4,230 / 1,820 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.02.5 / 1.2 | Impact X-Y / Z (ISO 179, unnotched)57.5 / 13.3 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)170 °C |
| PLA Basic | Our statusmost popular | Density (ISO 1183)1.24 g/cm³ | Bending modulus X-Y / Z (ISO 178)2,750 / 2,370 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.01.4 / 1.4 | Impact X-Y / Z (ISO 179, unnotched)26.6 / 13.8 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)54 °C |
| PETG HF | Our statusmost popular | Density (ISO 1183)1.28 g/cm³ | Bending modulus X-Y / Z (ISO 178)2,050 / 1,810 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.01.0 / 1.0 | Impact X-Y / Z (ISO 179, unnotched)31.5 / 10.6 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)62 °C |
| PC FR | Our statusmost popular | Density (ISO 1183)1.18 g/cm³ | Bending modulus X-Y / Z (ISO 178)1,890 / 1,660 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.01.0 / 1.0 | Impact X-Y / Z (ISO 179, unnotched)55 / 8.0 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)108 °C |
| ASA Aero | Our statusmost popular | Density (ISO 1183)0.99 g/cm³ | Bending modulus X-Y / Z (ISO 178)1,510 / 1,220 MPa | Stiffness per gram X-Y / Z, PETG HF = 1.01.0 / 0.9 | Impact X-Y / Z (ISO 179, unnotched)32.0 / 3.4 kJ/m² | Heat deflection, 1.8 MPa (ISO 75)78 °C |
The working: PETG HF gives 2,050 / 1.28 = 1,602 along the layers and 1,810 / 1.28 = 1,414 across them. PPA-CF gives 9,860 / 1.25 = 7,888 along the layers, and 7,888 / 1,602 = 4.9. Every other cell is the same sum. The ratios are rounded to one decimal and go no further than the datasheets allow.
Water, for a part that flies in rain: saturated absorption at 25 °C and 55% RH is 0.05% for PPS-CF, 0.37% for PET-CF, 1.30% for PPA-CF and 2.35% for PA6-CF. A PPA-CF part can change size slightly in a damp room; PET-CF takes up less than a third as much water.
Stiffer per gram, not lighter
The three carbon fibre grades on our most popular list are not lighter than PETG HF. At the same volume, PPA-CF and PPS-CF weigh 98% of PETG HF and PET-CF weighs 101%. The lightest grades in the table are ASA Aero at 0.99 g/cm³ and the carbon fibre nylons we order in, PAHT-CF at 1.06 and PA6-CF at 1.09.
What carbon fibre buys is stiffness at the same weight. Along the layers PPA-CF is 4.9 times PETG HF per gram, PPS-CF 3.5 times, PET-CF 2.6 times. So a PPA-CF arm of the same size as a PETG HF arm weighs about the same and bends about a fifth as much, or it can be made thinner for the same bend and weigh less. That second route is where the weight saving comes from, and it is a design decision, not a material property.
Print the arm flat
Across the layers most of the lead goes. PPA-CF keeps 1.8 times PETG HF's stiffness per gram in Z; PET-CF and PAHT-CF keep 1.2, below PLA Basic's 1.4. Printed standing up, with its layers across the bending, a PET-CF arm is less stiff per gram than the same arm in PLA Basic. So we print an arm lying flat, with the bending along the layers; we choose the print orientation. Say which way the load runs when you send the file.
Crashes load the layers too. Across the layers the carbon fibre grades on our most popular list give 2.8 to 4.5 kJ/m² unnotched impact (ISO 179); PA6-CF gives 15.5 and PAHT-CF 13.3, both ordered in, and PLA Basic 13.8. A part that must survive a crash either lies so the hit runs along the layers, where PPA-CF gives 41.7 kJ/m² and PAHT-CF 57.5, or it is a TPU part. A full table of X-Y against Z for 12 grades is on Layer strength: X-Y vs Z.
Light: ASA Aero, and what the datasheet cannot tell you
ASA Aero foams as it prints, and Bambu Lab's store copy names "weight-sensitive projects, such as RC planes" as its use. Its datasheet density is 0.99 g/cm³, the lowest on this page, and its bending modulus 1,510 MPa along the layers, so on the datasheet rows it is no stiffer per gram than PETG HF.
Read those rows with care. Bambu Lab printed the datasheet specimens at a 225 °C nozzle, below the 240-280 °C it recommends for printing, so the 0.99 g/cm³ and 1,510 MPa describe a bar that had barely foamed. Bambu Lab publishes no stiffness for a foamed print, and we promise no weight for one. Use ASA Aero where the shape is fixed and grams count, a canopy, a fuselage, a cover, a shell, not where an arm must not flex.
TPU for what hits
- TPU for AMS, Shore 68DLanding feet, bumpers, camera and antenna mounts that should keep their shape. One of our most popular materials. On its datasheet it breaks at 31% elongation across the layers with 9.6 kJ/m² impact there, against more than 650% and 124.3 kJ/m² along them, so a mount loaded along its layers is the design.
- TPU 95A HFDamping mounts, soft bumpers, straps and anything that stretches so its layers open: more than 480% elongation and 86.3 kJ/m² impact across the layers, and 22.3 MPa tensile strength there. Ordered in for the job; the quote gives the time.
- TPU 90A and TPU 85ASofter still. Bambu Lab places TPU 90A in "shoe soles, RC tires, and functional components that require both flexibility and strength". Both are ordered in. The four TPU grades print without a heated chamber, so a TPU part can be up to 340 x 320 x 340 mm in one piece. The full comparison is on TPU 3D printing.
Near the motors
Heat deflection at 1.8 MPa (ISO 75) is a short test on a loaded specimen, not a working temperature, but it ranks the grades: PLA Basic 54 °C, PETG HF 62 °C, ASA Aero 78 °C, PC FR 108 °C, PET-CF 182 °C, PPA-CF 196 °C, PPS-CF 235 °C. A motor mount or an ESC cover in PLA Basic is the part that sags first. No datasheet knows your motor's temperature; tell us what it reaches and a person checks the part against the number.
What we do not do
- Flight ratingWe do not certify parts for flight and hold no aviation approval of any kind. We print the part to the datasheet material you choose; whether the aircraft flies with it is your test.
- PropellersA propeller is the obvious question: no Bambu Lab datasheet gives a fatigue figure, and a printed part always has a weak direction across its layers. Send the file and say what it flies on, and a person answers before any price.
- A match for a laminated composite frameWe hold no figures for laminated composite plates or tubes, so we make no comparison with them. Send the drawing and a person says whether a printed part can do the job at all.
- Electronics on boardA box for a flight controller, a battery or a robot's electronics is a separate question: PC FR for a flame-retardant housing, PETG HF for the rest.
Send the frame file and say what it carries
Send the STEP or STL and say what the part does: an arm that carries a motor, a plate that holds the stack, a bumper that takes the landings. A person chooses the material and the print orientation, adds walls where the part carries load, and replies with a price in 3 hours on average on workdays.
- PPA-CF, PET-CF, ASA Aero and TPU for AMS: among our most popular materials, usually 2-5 working days after payment.
- PA6-CF, PAHT-CF and TPU 95A HF: ordered in for the job; the quote gives the time. Ask for two materials in one request and the quote prices each.
- Largest part in one piece: 340 x 320 x 340 mm in every material. Tolerance ±0.5%, minimum ±0.5 mm.
- A cheap first frame for a fit check: 24/7 PETG. Posted to the Baltics, Finland, Sweden and Denmark.
Questions
Checked by the druckworks workshopUpdated
Is carbon fibre filament lighter than PETG?
Not the ones we print most. On Bambu Lab's datasheets PPA-CF is 1.25 g/cm³, PPS-CF 1.26 and PET-CF 1.29, against PETG HF at 1.28 (ISO 1183); the carbon fibre nylons we order in are lighter, PAHT-CF at 1.06 and PA6-CF at 1.09. PPA-CF, PPS-CF and PET-CF are stiffer per gram, not lighter per volume; the weight saving comes from making the part thinner.
PPA-CF or PET-CF for a drone frame?
PPA-CF when it must be as stiff as possible: 9,860 MPa bending modulus along the layers against PET-CF's 5,320 (ISO 178). PET-CF when it flies in the wet: 0.37% saturated water absorption against 1.30%. Both are among our most popular materials.
Which TPU for drone mounts?
TPU for AMS, Shore 68D, for a mount that should hold its shape. TPU 95A HF for one that damps or stretches across its layers: more than 480% elongation there against 31% for TPU for AMS. The soft grade is ordered in.
Is ASA Aero good for RC planes?
Bambu Lab sells it for "weight-sensitive projects, such as RC planes" (its store page). Its datasheet density is 0.99 g/cm³, measured on a specimen printed below its recommended nozzle temperature, and Bambu Lab publishes no stiffness for a foamed print. We print it for shells and covers and promise no weight.
Can you print propellers?
No datasheet gives a fatigue figure for a spinning part, and FDM always leaves a weak direction across the layers. Send the file and say what it flies on; you have the answer before any price.
Do you certify parts for flight?
No. We hold no aviation approval and do not certify any part. We print the part in the material you choose; the flight test is yours.
How big can a frame be in one piece?
340 x 320 x 340 mm in PPA-CF, PET-CF, PPS-CF and ASA Aero, which need a heated chamber.
Send the frame file and say what it carries
Send the file and write what the part does and which way the load runs. A person picks PPA-CF, PET-CF, ASA Aero or TPU, chooses the print orientation and replies with a price in 3 hours on average on workdays.